Slump
The specimens were divided into two groups: a nano-SiO2 control group and a composite fiber control group. The slump values for each group are summarized in Fig. 5. In the nano-SiO2 group, the R100-W sample (recycled concrete without a…
The specimens were divided into two groups: a nano-SiO2 control group and a composite fiber control group. The slump values for each group are summarized in Fig. 5. In the nano-SiO2 group, the R100-W sample (recycled concrete without a…