Phase composition of porous bioceramics
The XRD patterns of the samples calcined at 400 °C are shown in Fig. 1a. The samples synthesised using calcium acetate (Ac3–Ac10) are less crystalline, with broader peaks and lower intensities compared to…
The XRD patterns of the samples calcined at 400 °C are shown in Fig. 1a. The samples synthesised using calcium acetate (Ac3–Ac10) are less crystalline, with broader peaks and lower intensities compared to…