Experimental study of the effect of seawater and temperature on the corrosion resistance of cement composites with the addition of copper post-flotation waste

Compressive strength of cement composites—temperature 10°C and 20°C

Figures 2 and 3 show the average compressive strength of cement composites without and with 2.5%, 5%, 7.5%, and 10% PFW in the water and seawater (3.3%) environments after…